http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002072533-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_20d3042eb4ea7c9afd525aa89373349d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 |
filingDate | 2000-09-04-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_caa57a299ef1588e1f8f27b833559fe2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_df4dfa72151c0f9c0bba372113296acf http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_87d0076b51b9d04a83f624c81cd61692 |
publicationDate | 2002-03-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002072533-A |
titleOfInvention | Toner for developing electrostatic images |
abstract | [Problem] To provide an oilless method as a heat roller fixing method, to obtain a good fixing property, and to be excellent in developing characteristics, transfer efficiency, resolution, gradation, etc., spherical to approximately. Provided is a toner for developing an electrostatic image composed of a spherical polyester resin. SOLUTION: It contains a binder resin composed of an acidic group-containing polyester resin (I), a coloring agent, and a release agent melt-blended with the polyester resin (II). Perimeter of a circle with the same area as the area) / (Circumferential length of projected particle image) is 0.97 or more. |