Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_758994071efb42b565fc2c04637be131 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02E60-13 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-58 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-80 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G11-78 |
filingDate |
2001-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b664d17af5bc0a29aecd2afbaad27d31 |
publicationDate |
2002-02-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2002064037-A |
titleOfInvention |
Electrode coating agent and electric double layer capacitor using the same |
abstract |
(57) [Problem] To provide an electrode coating agent for reducing leakage current without lowering capacitance. SOLUTION: An electrode coating material (B) containing an electrochemically polymerizable monomer (A) is used. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005310702-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013503244-A |
priorityDate |
2000-06-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |