http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002054089-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_561b303fd100fe27818524fd5b083df8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H27-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-34 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-60 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F220-56 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H21-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D21H19-20 |
filingDate | 2000-05-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5a9f4f29c36d5061f1534919583cda7a |
publicationDate | 2002-02-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002054089-A |
titleOfInvention | Manufacturing method of laminated paper |
abstract | PROBLEM TO BE SOLVED: To provide an interlayer adhesive in the production of a laminated paper, in which an ion complex is formed and then added to a paper layer by spraying, the apparent viscosity is low and spraying is easy. The present invention provides a polymer substance having a sufficient adhesive strength and a method for producing a high-strength laminated paper by using the same. SOLUTION: A primary amino group-containing amphoteric polymer produced by polymerizing a monomer mixture containing a primary amine-containing acrylic cationic monomer and a carboxyl group-containing anionic monomer as essential components is converted into a paper. In the method for producing two or more layers of laminated paper including the steps of pressing after laminating after forming the layer and further drying, spray-adding to the wet paper layer after laminating and before laminating. Can be achieved by: |