http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002020215-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_e9a25524a7966900de2731d0b4e30cba |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61C13-007 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61C13-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-07 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61K6-00 |
filingDate | 2000-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d24bba99f74f75e4448ef2803a9ae1ce |
publicationDate | 2002-01-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002020215-A |
titleOfInvention | Silicone rubber, product using the same, and manufacturing method |
abstract | (57) [Problem] To provide a denture in which silicone rubber is lined on a surface of a denture base to be worn on a human body. SOLUTION: A wax 3 having a predetermined thickness is applied to a surface of a denture base 2 made of PMMA on a side to be attached to a human body, and a denture 1 is fixed in a lower flask 5 with gypsum 6 so that the wax 3 surface is exposed. I do. When closing the upper and lower flasks 4 and 5, The plaster 6 is poured into the upper surface of the denture base 2 including the wax 3 and left to harden the plaster 6. Then, the flasks 4 and 5 are opened, the wax 3 is washed away with a solvent, the denture base 2 is treated with dichloromethane and dried, and a suitable amount of the silicone 8 to which a small amount of MMA has been added is applied from above the denture base 2. pour it up. The flasks 4 and 5 are closed and transferred into a pressure cooker and heated at about 3 atm at about 50 ° C. for 24 hours. Thereby, at the same time as the polymerization of the silicone rubber, the polymerization of the MMA also proceeds near the surface, which contributes to the strong adhesion of the PMMA to the denture base 2 to obtain the denture 1 with the soft silicone rubber 9 lined. . |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111154210-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009122499-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008073229-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6805556-B2 |
priorityDate | 2000-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 25.