Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-32 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K3-38 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-55 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G64-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-524 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-521 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-103 |
filingDate |
2000-06-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_620909bc47401127f9c502a296289195 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_af0a73aa5393149d4497733eac215298 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_867c4c8e92db9ddf90a7710634553b5b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5329691231c5363be1a4473de4a57237 |
publicationDate |
2002-01-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2002012756-A |
titleOfInvention |
Method for producing polycarbonate resin composition |
abstract |
(57) [Problem] To produce a polycarbonate resin composition having moldability and heat stability. SOLUTION: A sulfonic acid compound is added to an aromatic polycarbonate obtained by polycondensation of an aromatic dihydroxy compound and a carbonic acid diester in the presence of a specific catalyst, and a melt viscosity change rate is 0.5% or less, and a terminal is added. Hydroxyl group amount 100eq After obtaining an aromatic polycarbonate composition (A) of not more than / ton, at least one hydroxyl group contains an ester of a long-chain fatty acid having 8 or more carbon atoms in 100 parts by weight of the aromatic polycarbonate composition (A). A compound (C) 0 selected from 0.001 to 0.5 parts by weight of a long-chain fatty acid ester (B) of a polyhydric alcohol having 2 to 20 carbon atoms and an inorganic acid and a partial ester of an inorganic acid. . 0001-0.01 parts by weight are added. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009072671-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011256359-A |
priorityDate |
2000-06-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |