http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002003814-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_20d3042eb4ea7c9afd525aa89373349d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J175-04 |
filingDate | 2000-06-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b37c78324955db419f3cfc5d2c506d65 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8fae1b2d8084ce6440dc7414044002ee |
publicationDate | 2002-01-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002003814-A |
titleOfInvention | Adhesive composition |
abstract | PROBLEM TO BE SOLVED: To combine white ink properties and adhesive properties, especially to improve adhesion after heat sterilization, reduce the number of colors in the printing process, and increase concealment. And an adhesive composition for lamination. SOLUTION: The glass transition point is -10 ° C to 30 ° C, the carbon ring concentration including alicyclic ring and aromatic ring is 1.0 to 4.0 mmol / g, the number average molecular weight is 500 to 16000, 2. A laminating material comprising: a main agent containing a kneaded mixture of a polyol having a Gardner color number of 3 or less and a white pigment; and a curing agent containing a polyisocyanate. Liquid mixed adhesive composition. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019099629-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008058703-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20200081762-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102250571-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8455101-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-102256924-B1 |
priorityDate | 2000-06-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 166.