http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002001808-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ad2cd796f8c4dcb425ddcc68707d3444 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L67-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 |
filingDate | 2000-06-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d76ef9bd0b27217895630ad71f60f812 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d0f530f8b102a50648526305ff8e95af http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d3091a214a72cde00f159621da8d9b20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5b5473ac83af9ed70a18307988ffa70b |
publicationDate | 2002-01-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2002001808-A |
titleOfInvention | Biaxially stretched polyester film and method for producing the same |
abstract | (57) [Summary] [PROBLEMS] While maintaining mechanical properties, fragrance retention, heat resistance, oil resistance, low moisture absorption, and dimensional stability under dry heat and wet heat environment required especially for food packaging materials, An object of the present invention is to provide a biaxially stretched polyester film having excellent tear straightness and excellent tear stability. SOLUTION: The biaxially stretched polyester film having a linear tear property in which the angle between the cut surface after tearing and the acute angle side formed by the film surface is not less than 20 degrees and less than 90 degrees in both the machine direction and the direction perpendicular to the film production. It is. |
priorityDate | 2000-06-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 50.