http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001353830-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_997ed5b3b186e8e8ddd4b0f8685a1d12 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-524 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L69-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B27-36 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-14 |
filingDate | 2000-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_92f29c9502b6a53a20e0ed259543ff08 |
publicationDate | 2001-12-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001353830-A |
titleOfInvention | Polycarbonate resin laminate |
abstract | (57) [Problem] To provide a polycarbonate resin laminate excellent in strength characteristics with little distortion even when the laminate is molded by a method such as insert molding. A component having a molecular weight of 3,000 or less in terms of monodisperse standard polystyrene measured by a GPC (gel permeation chromatography) method has an area ratio of 3 to 3 in a GPC chart having a logarithm of the molecular weight on the horizontal axis. 15% and its weight average molecular weight is 30,0 A layer (A layer) composed of a polycarbonate resin (component A) having a weight average molecular weight of 50,000 to 45,000, as measured by GPC laminated on the layer A; A polycarbonate resin laminate comprising a layer (B layer) composed of 0 to 80,000 polycarbonate resin (B component). |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011068123-A |
priorityDate | 2000-06-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 404.