Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_9592efd24c0c67b5f1b405d7d0c0c29a http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dc45703f67bc72a6db582867886fd5d5 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-21 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-3472 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L61-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B22C1-22 |
filingDate |
2000-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bde5a25b01460ef9a2d2adcb8e176366 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_584d53db6c736c47a108c6b83d72b1b6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_72c042e7e3ae3480cc64f4a657bcd8ce |
publicationDate |
2001-11-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2001321883-A |
titleOfInvention |
Binder for shell mold and method for producing the same |
abstract |
PROBLEM TO BE SOLVED: To provide a shell mold binder in which a core is prevented from cracking at the time of casting a light alloy, and furthermore, the generation of formaldehyde during the molding of the shell mold is suppressed. SOLUTION: The mass average molecular weight measured by gel permeation chromatography is 1000 or more, and the relative retention ratio to the phenol peak is 0.80 to 0.80. The ratio (I / II) of the peak height I of 0.81 to the peak height II of 0.75 to 0.79 is 1.0 or more, and the gel time at 150 ° C. according to JIS-K6910 is 30. It is a binder for shell mold mainly composed of bisphenol A-modified novolak phenol resin for up to 60 seconds. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7579075-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2019142488-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-WO2019142488-A1 |
priorityDate |
2000-05-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |