http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001302738-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dbdfa36b677f4ef61245ca725011e221 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G65-48 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F283-08 |
filingDate | 2000-04-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_05512de9f49acb559654296c08f55e8a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_34086429b7516256788f6a901d962ce7 |
publicationDate | 2001-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001302738-A |
titleOfInvention | Method for producing novel functionalized polyphenylene ether resin and composition thereof |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a functionalized polyphenylene ether resin which is sufficiently functionalized, has excellent workability, has a good balance of color tone and appearance, heat resistance and mechanical properties, and sufficiently satisfies the demands of the industrial world. provide. SOLUTION: The molecular structure has at least one carbon-carbon double bond or triple bond and at least one glycidyl group per 100 parts by weight of polyphenylene ether (A) comprising a structural unit of the formula (1). At least one A mixture containing 0.01 to 50.0 parts by weight of a kind of the functionalized compound (B) is reacted at a reaction temperature of 50 to 150 ° C. and in a system substantially free of a solvent. A method for producing a polyphenylene ether resin. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-02059180-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6835795-B2 |
priorityDate | 2000-04-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 56.