http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001296632-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_13aa7b32ae00ed83af7dfaa0b6a1f7c2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-498 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-08 |
filingDate | 2000-04-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e271f7b3c2437de1aa9f100c01530e02 |
publicationDate | 2001-10-26-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001296632-A |
titleOfInvention | Photothermographic material, image recording method and image forming method using the photothermographic material |
abstract | (57) [Problem] To provide a photothermographic material having high sensitivity, low fog, and excellent silver tone and image storability. Provided are an image recording method and an image forming method using the photosensitive material. SOLUTION: The composition contains at least a non-photosensitive organic silver salt, a photosensitive silver halide, a reducing agent capable of reducing silver ions of the organic silver salt to silver when activated by heat, a binder, and a cross-linking material of the binder. (1) the photosensitive silver halide contains at least one transition metal selected from the elements of Groups 6 to 11 of the periodic table; The hydrophilic colloid contained in the photosensitive silver halide is 40 g or less per 1 mol of silver; (3) the hydrophilic colloid is 6 × 10 6 g or more per 1 mol of the transition metal; A photothermographic material characterized by satisfying the following conditions: |
priorityDate | 2000-04-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |