http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001294784-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_905122d8678a831c0f8af203f34145dc |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41M5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B41J2-01 |
filingDate | 2000-04-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_11a5f087f39c148a597efc6dfc0e7c8d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d8d2e542d7256401cc132418a9e1503f |
publicationDate | 2001-10-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001294784-A |
titleOfInvention | Hot melt ink |
abstract | PROBLEM TO BE SOLVED: To provide a hot-melt ink excellent in acid resistance and alkali peeling property and suitable as a mask for an electronic circuit board. SOLUTION: The hot-melt ink of the present invention has a wax having an acid value of 80 or more (for example, montanic acid wax) 82.9. % By weight, and 15% by weight of a wax having a branched molecular structure (for example, microcrystalline wax, oxidized microcrystalline wax, low-density polyethylene wax, or oxidized low-density polyethylene wax); 0.1% by weight of antioxidant and 2% by weight of dye By stirring at a temperature of. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011243985-A |
priorityDate | 2000-04-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 28.