http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001294684-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_dbdfa36b677f4ef61245ca725011e221 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01J47-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L29-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B01D71-38 |
filingDate | 2000-04-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_34703de68226773060cb682e1341d81b |
publicationDate | 2001-10-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001294684-A |
titleOfInvention | Heterogeneous ion exchange membrane and method for producing the same |
abstract | PROBLEM TO BE SOLVED: To provide a heterogeneous ion exchange membrane having excellent ion selectivity and fouling resistance while keeping the electrical resistance of the membrane low, and a method for producing the same. SOLUTION: This is a heterogeneous ion exchange membrane comprising fine particles of an ion exchange resin and a binder resin, wherein the binder resin is a heterogeneous ion exchange membrane containing an ethylene-vinyl alcohol copolymer. A binder resin powder containing a vinyl alcohol copolymer is mixed in advance at a temperature lower than the lowest melting point of the binder resin component, and is heated and kneaded. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5942267-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112691550-A |
priorityDate | 2000-04-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 21.