http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001254231-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ff2c56f436be89e332c32a0ea17186ec |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A61L15-16 |
filingDate | 2000-03-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_568611f3438853642df5a3bd77d9a053 |
publicationDate | 2001-09-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001254231-A |
titleOfInvention | Chitin fiber and method for producing the same |
abstract | (57) [Summary] [Problem] To obtain chitin fiber that is hardly melted in a living body, to obtain a chitin fiber aggregate from such fiber, to obtain a medical material from the chitin fiber aggregate, and to obtain a chitin fiber aggregate It is an object of the present invention to obtain a wound covering and protecting material from. SOLUTION: In producing chitin fibers by wet spinning chitin, it has been found that when chitin having a specific molecular weight is used, it is difficult to melt when used in a living body, and that chitin fibers which have not been obtained conventionally can be obtained. confirmed. That is, in producing chitin fibers, chitin having a solution viscosity of 30 to 48 ° C. and a concentration of 2-48 centipoise when dissolved in a dimethylacetamide solution containing 8% by weight of lithium chloride is used. And a method for producing chitin fibers, and chitin fibers obtained by such a method. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-102888672-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-101036799-B |
priorityDate | 2000-03-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |