http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001248036-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d0ae9df648bfc0aa046910361c967ca2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02G3-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D03D15-00 |
filingDate | 2000-03-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_02ccd39b80e155d8f88f206b3fa5ec90 |
publicationDate | 2001-09-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001248036-A |
titleOfInvention | Manufacturing method of long and short composite fabric |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a stretchable short and long composite fabric having the softness and swelling of wool fiber and the resilience, wrinkle resistance and moderate drape of polyester filament yarn. provide. SOLUTION: The weight ratio of a latently crimpable polyester filament yarn obtained by compound-spinning two kinds of polyester polymers having different heat shrinkage characteristics and a wool spun yarn made of wool fiber is 30/7. After weaving the long and short composite plied yarns that have been plied by setting the twist coefficient K according to the following equation to 2.9 to 4.2 so as to be 0 to 50/50 as the weft of the woven fabric, the mixture is stirred by liquid flow. In this way, a finishing process including a step of developing elasticity in the lateral direction is performed. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-104294455-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012102445-A |
priorityDate | 2000-03-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 21.