http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001234120-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2dcebf5a7f7ddc3b081f70e8ce1c4097 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_ec032d3f96e5e01e66762cc63f12b572 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D175-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-14 |
filingDate | 2000-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_005fb927391d94d54c36815c71cef35c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a8818974fad9efc03524e3566fd608a2 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_65462e828de6a244404efbae8897d313 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9e64964bd6b48b346450b7e25d0266ae |
publicationDate | 2001-08-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001234120-A |
titleOfInvention | Paint for metal plate, coated metal plate and method for producing the same |
abstract | (57) [Abstract] [Problem] To paint on a metal plate to give a textured uneven pattern, to provide a coating film with good physical properties and to be resistant to scratches, electric equipment, indoor equipment, vehicle interiors, architecture. Provided are a coated metal plate formed by applying the paint which can be suitably used for interior decoration and the like, and a method for manufacturing the coated metal plate. A resin forming a film having a breaking elongation of 40 to 200% and a breaking tensile strength of 8 to 40 MPa obtained by the reaction of a polyol resin (A) and a block type polyisocyanate compound (B), and a resin solid content of 100 0.05 to 10 parts by weight of heat-expandable microcapsules with respect to parts by weight (C), and a metal plate paint containing at least one organic solvent (D) selected from aromatic hydrocarbon-based, alcohol-based, ether-based, and ester-based solvents; And a method for producing a coated metal sheet by applying the coating material to the metal sheet and heating the metal sheet for 20 to 180 seconds so that the metal sheet temperature reaches 100 to 260 ° C. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2012210722-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015147863-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009263571-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-6908951-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4560297-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013018897-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005206736-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004182284-A |
priorityDate | 2000-02-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 88.