http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001233921-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_c62268de3e92657ca5b9adcac4778225 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F236-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F8-04 |
filingDate | 2000-02-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_374fa4872a7d430968c0efc2355e0156 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fbdf64ecf3d1a59ccf92259168281f86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c39331a2c0d099200ccd21656d3d1025 |
publicationDate | 2001-08-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001233921-A |
titleOfInvention | Polymer and method for producing the same |
abstract | (57) [Problem] To provide a method for improving cold resistance of a chloroprene polymer. SOLUTION: In the method for forming a carbon-carbon bond by adding hydrogen to a double bond present in a chloroprene polymer, a specific hydrogenation catalyst is used, and the hydrogenation reaction is carried out in the polymer during the hydrogenation reaction. By setting the existence ratio of microstructure units to be generated in a specific range, A polymer having a glass transition temperature Tg in the range of −40 ° C. to −80 ° C. while maintaining a rubber-like elastic body, and having drastically improved cold resistance. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110498880-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002060419-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-110498880-B |
priorityDate | 1999-12-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 108.