http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001233902-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7f9af914ed2fb00cd4f1b8b1a28964e4 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P20-141 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-01 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F2-32 |
filingDate | 2000-12-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5aea6adbfabc04066f3fbcd6fc43c8ed http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ac276acd71213f6d19bbf0eb6de530fc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_4cdc4d85ca45d4e7237ff15ab7c3e694 |
publicationDate | 2001-08-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001233902-A |
titleOfInvention | Method for producing porous crosslinked polymer |
abstract | (57) [Summary] [PROBLEMS] A water-in-oil type high dispersion phase emulsion (hereinafter referred to as HI) The present invention provides a method for producing a HIPE polymer while preventing leakage of PE, increasing the thickness and maintaining the thickness including both ends, preventing unpolymerization by reducing oxygen, and holding a sheet such as an upper film. A method for producing a porous cross-linked polymer by horizontally and continuously polymerizing HIPE, wherein weirs are used at both ends in the width direction of a support of the HIPE used for horizontally and continuously polymerizing the HIPE. A method for producing a porous cross-linked polymer, characterized by the following. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-111135999-A |
priorityDate | 1999-12-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |