http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001224868-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f33bb47e111726802f48d2a0f830a2e8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A63H33-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L25-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A63H9-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L53-02 |
filingDate | 2000-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b7cd04285f1118a9e771d5e71b942b75 |
publicationDate | 2001-08-21-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001224868-A |
titleOfInvention | Resin material for toys |
abstract | (57) [Summary] [PROBLEMS] The present invention not only has the same features in price and workability as compared with vinyl chloride resin, but also It is an object of the present invention to provide a resin material that does not generate endocrine disrupting chemical substances or dioxins at the time of use or disposal and that is suitable for toys. SOLUTION: The present invention relates to a styrene-butadiene block copolymer (SBS) in the form of pellets or powder having a particle size of 20 to The mixing ratio of 70% by weight and the styrene resin is appropriately adjusted within the range of 80 to 30% by weight, and they are mixed by heat melting to form a polymer alloy or a polymer blend. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008069189-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2008032556-A1 |
priorityDate | 2000-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 32.