http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001220483-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_a8cde4f2bd60df7888c8040bdfcc8a5d |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L29-04 |
filingDate | 2000-02-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b3730e36b0057fb6dee591de675af53c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7da48e6c0599ad594f5b7c6f2d12d155 |
publicationDate | 2001-08-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001220483-A |
titleOfInvention | Polyvinyl alcohol resin composition |
abstract | (57) [Summary] [PROBLEMS] To provide a polyvinyl alcohol-based resin composition which does not cause yellowing or off-flavor during high-temperature heat treatment. SOLUTION: The polyvinyl alcohol resin (A) comprises a polyvinyl alcohol resin (A) and a hydrazine compound (B), and the content of the hydrazine compound (B) is polyvinyl alcohol resin (A). 0.005 to 20 parts by weight per 100 parts by weight. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015120823-A |
priorityDate | 2000-02-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 106.