http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001215653-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-498 |
filingDate | 2000-09-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c1fef7c760fc1e2ee4c255680342f7fa http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_77d0592288a3b52e157a1c227fbea5f9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b37c64d819ea8962054cb6f623542351 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d2f196bdee5ae2426622693845dfe62f |
publicationDate | 2001-08-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001215653-A |
titleOfInvention | Photothermographic material |
abstract | PROBLEM TO BE SOLVED: To provide a photothermographic material which gives a sufficient image density within a realistic reaction temperature and reaction time and suppresses coloring of a white background when stored for a long time after development processing. thing. A photothermographic material containing a photosensitive silver halide, a non-photosensitive organic silver salt, a reducing agent for silver ions and a binder on at least one surface of a support, wherein the photothermographic material is A photothermographic material, wherein at least one of the constituent layers contains an oxazoline compound. |
priorityDate | 1999-11-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |