Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationCPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2913 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2924 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y10T428-2969 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D02G1-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01D5-082 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/D01F6-92 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02G3-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D03D15-567 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02G3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01D5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02G1-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02J1-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D02J1-22 |
filingDate |
2000-10-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1853d30cbe9b17d9eea5115db338f55f http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ed28bf78cdb6abe9990b714a49a770c5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ff55cdabd87793fa9eadb5bf49d1fc59 |
publicationDate |
2001-07-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2001192942-A |
titleOfInvention |
Bulky yarn and method for producing the same |
abstract |
PROBLEM TO BE SOLVED: To provide a bulky processed yarn having a large difference in yarn foot with no displacement of a sheath yarn and a large swelling, and a method for producing the same. Filament yarn (FY), one of FY (FYA) and the other FY (FYB) are partially mixed and entangled, and the average yarn length of FYB is 8 to 40% longer than that of FYA. coefficient of variation of the yarn length between the filaments (CV a%) At most 3% and F between filaments constituting FYB. The coefficient of variation of the yarn foot difference with respect to the average yarn length of YA (CV BA %) Is in the range of 10 to 20%. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2008223166-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2010133052-A |
priorityDate |
1999-10-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |