Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_2cb72657cf0479385a9b5e655af1e16f |
classificationIPCAdditional |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29K23-00 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C51-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-642 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F4-6592 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F110-06 |
filingDate |
2000-01-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a623693a657104afbe92ce09199e511b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_fb4815583e2d7a4f3008ca1cc59ff9ad |
publicationDate |
2001-07-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2001192412-A |
titleOfInvention |
Propylene homopolymer, thermoplastic resin composition and molded article |
abstract |
PROBLEM TO BE SOLVED: To provide a propylene homopolymer in which glass transition temperature is effectively reduced, embrittlement at a low temperature is suppressed, and impact resistance is improved. SOLUTION: The intrinsic viscosity [η] measured in a tetralin solvent at 135 ° C. is 0.005 to 20 deciliter / g, and the formula (I) is determined by 13 C-NMR measurement. Is a propylene homopolymer having an index K value of the polymer chain structure of 2.0 or more. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2006045457-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1464657-A1 |
priorityDate |
2000-01-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |