http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001154310-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_13aa7b32ae00ed83af7dfaa0b6a1f7c2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-498 |
filingDate | 1999-11-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d9c5e6733e9051638dd2ead8319f88b6 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dbac48077338c1955bee6bcf3f266565 |
publicationDate | 2001-06-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001154310-A |
titleOfInvention | Photothermographic material and image forming method |
abstract | An object of the present invention is to provide a photothermographic material excellent in fog density and color tone stability in thermal development and an image forming method. SOLUTION: In a photothermographic material containing at least a non-photosensitive organic silver salt and a photosensitive silver halide, a density fluctuation ratio 1 represented by the following formula (1) is 1.00 or less. Photothermographic material. Equation (1) Density fluctuation ratio 1 = ΔD temp1 / ΔD time1 In the equation, ΔD temp1 is the development temperature 12 at the reference development time. It represents the range of concentration fluctuation between 3 ° C and 124 ° C, and ΔD time1 is 1 It indicates the density fluctuation width between the reference development time at 23 ° C. and the development time longer by 1 second. |
priorityDate | 1999-11-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |