http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001150476-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d93502a23a72b56472bc75854cfe7c60 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E03C1-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C45-00 |
filingDate | 2000-02-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6fc7c49373411ebe4bd97de5b64491e8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_adee10db794ce7eced2a109ce3e85da8 |
publicationDate | 2001-06-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001150476-A |
titleOfInvention | Method for producing molded article and large molded article |
abstract | PROBLEM TO BE SOLVED: To provide a method for producing a molded article made of a polynorbornene-based resin, which does not substantially generate odor derived from unreacted monomers and the like, at a simple and low cost. I do. SOLUTION: After obtaining a molded body made of polynorbornene-based resin by subjecting a reaction stock solution containing a norbornene-based monomer to reaction injection molding, this molded body is subjected to a heat treatment at a temperature of 50 to 90 ° C. In the heat treatment, it is preferable that heating by air flow is performed in an oven for 0.1 to 5 hours. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003039475-A |
priorityDate | 1999-09-16-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 47.