http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001131532-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_6c8d4dc7bd1a30d8fda907fceaeb4e69 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J201-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J123-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09K3-10 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J123-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D65-40 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D77-20 |
filingDate | 1999-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b021d37da6fa836cc761b257f6ef5926 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5cde30009fda9f37eed3ff87129a0ded http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8764846ee2b6e138374ffe75a316cd8d |
publicationDate | 2001-05-15-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001131532-A |
titleOfInvention | Sealant composition having easy peelability and easily openable container |
abstract | PROBLEM TO BE SOLVED: To provide a seal having appropriate strength at the time of heat sealing, to be able to easily open (peel) at the time of opening (peeling) after joining, to have low-temperature heat sealability and heat sealing. Provided is a sealant composition having good heat resistance in a part. A sealant composition having easy peelability comprising a composition comprising the following components (A) and (B) and satisfying the condition (C). (A) a modified olefin polymer modified with an unsaturated carboxylic acid anhydride and an unsaturated carboxylic acid ester, wherein the average number of carboxylic acid anhydride groups per molecule is one or more, and In the modified olefin polymer, the ratio of the number of carboxylic acid ester groups to the number of carboxylic acid anhydride groups in the modified olefin polymer is 0.5 to 20, and the average number of hydroxyl groups per molecule of the modified olefin polymer (B) is 1 or more. The ratio of the number of hydroxyl groups of component (B) to the number of carboxylic anhydride groups of component (A) is 0.1 to 5; |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5872129-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2015166657-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2019038929-A |
priorityDate | 1999-11-05-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 87.