http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001122258-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_8c5803f5ec5dec7295046f3953c92d53 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D8-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D17-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B65D43-00 |
filingDate | 1999-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_31294dcba243fea3bdd550779983959c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9e5c552f504670ce88cfae04e9bd346a |
publicationDate | 2001-05-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001122258-A |
titleOfInvention | Laminated lid and method of manufacturing the same |
abstract | PROBLEM TO BE SOLVED: To provide an opening / feather without delamination or feathering when opening a score by cutting a score by pushing a tip of an opening tab or tearing off an opening. Excellent ring properties, workability and corrosion resistance, The objective is to supply a can lid that has a small environmental load and is excellent in the working environment during manufacturing. SOLUTION: In a resin laminated lid having a scored portion, a polyester resin layer is provided at least on the inner surface side of the can, and the molecular weight of the polyester resin of the inner surface resin layer in a portion along the scored portion is 25,000 to 70. 000 in the range of 000. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002211602-A |
priorityDate | 1999-10-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 73.