http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001121560-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_cb6b17f587d78ff76929032bcd5973bb |
classificationIPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29L7-00 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L47-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L83-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L1-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-20 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-28 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 |
filingDate | 1999-10-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cb6fa5cbe244317ba895b413ecca9370 |
publicationDate | 2001-05-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001121560-A |
titleOfInvention | Thin film manufacturing method and its manufacturing apparatus |
abstract | PROBLEM TO BE SOLVED: To provide a thin film manufacturing method and a manufacturing apparatus which can be easily mass-produced. SOLUTION: Water which is a non-solvent flows in through an inlet 11, By hitting the first buffer plate 121 and the second buffer plate 122, the water speed is reduced and turbulence does not occur. Water is buffer plate set 12 After passing through the forming tank 3, the flow guide plate set 31 Flows along the flow path and does not generate turbulence. At this time, the polymer solution is injected into a stable water flow of the molding tank 3 by the metering pump 22, and the polymer solution is guided and diffused by the flow guide plate set 31. Since the polymer solution does not dissolve in water and has a relatively high surface tension, the polymer solution diffuses on the surface of water to form a polymer thin film. The nonwoven fabric 320 is laid under the thin film, and the thin film is wound up with the nonwoven fabric 320 by the second roller 324. Since moisture and a solvent are attached to the wound nonwoven fabric 320 and the thin film, the drying device 35 is installed to set the nonwoven fabric 320 And, the moisture and the solvent contained in the thin film are dried to facilitate the storage of the thin film. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-101155925-B1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-112593323-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-8574783-B2 |
priorityDate | 1999-10-25-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 33.