http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001098135-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L51-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08F255-02 |
filingDate | 1999-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_825057ae673a371ee37b6fa4ba5ca0ab http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_818fe01176d81b024d3fdb9bd5ab55bd http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b6b3b102dc358649a69318b74c02d74e |
publicationDate | 2001-04-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001098135-A |
titleOfInvention | Vinyl compound-modified ethylene polymer composition, resin modifier comprising the composition, thermoplastic polymer composition, and molded article comprising the composition |
abstract | (57) Abstract: The composition of the present invention has [I] an intrinsic viscosity [η] in the range of 0.01 to 10 dl / g, an ethylene content of 35 to 75 mol%, and Ethylene polymer (A) for which no crystal melting peak is observed by the DSC method A vinyl compound-modified ethylene polymer obtained by graft polymerization of an aromatic vinyl compound or the like in a plug flow type reaction vessel, and a [II] density of 0.86 to 0.96 g / cm3 ethylene polymer and [III] glass transition temperature It contains a thermoplastic polymer having a (Tg) of 30 ° C. or higher at a specific ratio, and can be used as a resin modifier. The thermoplastic polymer composition of the present invention comprises the above [I] to [III], [IV] It comprises a thermoplastic polymer having a glass transition temperature Tg of less than 30 ° C, and can be used as a molded article. According to the present invention, it is possible to provide a molded article having an excellent balance between rigidity and surface hardness and impact resistance. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015147893-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014156548-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014177622-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014156547-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2014177623-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2014126215-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9657169-B2 |
priorityDate | 1999-09-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 257.