http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001089485-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_01c1e0bc0628f76dea731cda5a666ca1 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C07F7-08 |
filingDate | 1999-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f2bf2e0703e2137d3cfd8c0ae04fdecc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0486b462d0f9168026b7ceb19567a440 |
publicationDate | 2001-04-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001089485-A |
titleOfInvention | Curing agent, method for producing curing agent, and curable composition |
abstract | PROBLEM TO BE SOLVED: To provide a curing agent having good moldability, good compatibility with a highly polar carbon-carbon double bond-containing compound, and exhibiting sufficient cured material properties, and a curable composition. Providing things. SOLUTION: The following general formula (I) (A is a siloxane residue having at least one SiH group, B is a compound having 2 to 2 carbon atoms) 18, Y represents a covalent bond or a divalent organic group having 1 to 15 carbon atoms, Z represents a divalent organic group having 2 to 15 carbon atoms, and n represents 1 to 5; A curing agent represented by The curing agent comprises a carbon-carbon double bond-containing oligoester compound and two or more sulfur atoms per molecule. After the reaction with polysiloxane containing iH group, It is produced by reacting to leave a group. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007186482-A |
priorityDate | 1999-09-22-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 129.