Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1af8df51ce24ca931ae718fb747f6aa0 |
classificationCPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-1137 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-1135 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-1131 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-1138 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-1136 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-1075 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/G03G9-1139 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G15-09 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G15-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-113 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-107 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03G9-087 |
filingDate |
2000-05-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2da22582f652481974cc8012598f2a31 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_f3a1dce242838c5cdb1334e177920334 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_34d0c4f92b253f0776519141c2c9d66a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_72205e830d3b441f90d33e47b508eb14 |
publicationDate |
2001-03-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2001075315-A |
titleOfInvention |
Magnetic material-dispersed resin carrier, two-component developer, and image forming method |
abstract |
(57) [Problem] To provide a magnetic material-dispersed resin carrier excellent in environmental stability and long-term durability. SOLUTION: In a carrier core in which metal compound particles are dispersed in a binder resin and a magnetic material-dispersed resin carrier having a resin for coating the surface of the carrier core, the carrier has a temperature of 30 ° C. and a relative humidity of 80%. The amount of water adsorption T H2O-H (% by mass) after being left in the environment and the temperature of the carrier at 23 ° C. Moisture adsorption amount T H2O-L after being left in a 5% RH environment (mass%) And the surface area Sm (cm 2 / g) of the carrier have the following relationship: Is satisfied. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2009294253-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9958809-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2007017838-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2016147635-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9785070-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2011197568-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-10007206-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9500975-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4590319-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2003107777-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2990874-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2016170298-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-2913715-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-9599920-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015179258-A |
priorityDate |
1999-06-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |