http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001040316-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_d93502a23a72b56472bc75854cfe7c60 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09J157-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A47G27-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L101-02 |
filingDate | 1999-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_5181877d20a6c60beab58e778ecb584c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8a96cf80adfe9d83a891c41b1ea06bf1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3a2f4c24ad897e9622c61726d1004ad5 |
publicationDate | 2001-02-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001040316-A |
titleOfInvention | Latex for resin adhesive for carpet |
abstract | PROBLEM TO BE SOLVED: To provide a carpet excellent in moldability, thermoformability, heat-resistant shape retention and rigidity, and a latex for a resin adhesive for a carpet used in the production of the carpet. An acid group-containing ethylenically unsaturated monomer unit is provided. A latex of a copolymer comprising 30% by weight and 70 to 95% by weight of an olefin monomer unit copolymerizable therewith, wherein the glass transition temperature of the copolymer is 100 to 15%. Use a latex for carpet resin adhesive at 0 ° C. A carpet containing the latex for resin adhesive for carpet is obtained. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-2019105420-A1 |
priorityDate | 1999-07-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 90.