http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001031814-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_424db9d56b06a23aed410fcf5df652f3 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L45-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J3-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-5415 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K5-54 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/F16F15-08 |
filingDate | 1999-07-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c36fc09b5b8a3bbbdf8ad8ee8319a3f9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b00a5a564ca6fce002d1a3ded1f7861a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1cff3a340e965921011298fb3bc37855 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6fb243c675271cceaf8d7edf8d993d19 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ac8747ce4ef43a909710a8dd759932c8 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c45dbda5d1672050b13c73680b237988 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7ab4546dbf27db69c927e3daab17da5d http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_936844f9c0f3dc281a10f9ffedbf2277 |
publicationDate | 2001-02-06-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001031814-A |
titleOfInvention | Crosslinkable rubber compositions for vibration damping rubber and glass run and their uses |
abstract | (57) [Summary] A crosslinkable anti-combustion comb composition and a glass run comb composition of the present invention are crosslinkable by hot air and hot press, and the hot air crosslinked comb sheet has a pencil hardness of HB pencil. The test shows no scratches on the surface, the compression set after heat treatment at 150 ° C for 22 hours is 70% or less, and the hot-press crosslinked comb sheet has a tensile strength of 5 to 16 MPa and 150 ° C for 22 hours. The compression set after heat treatment is 70% or less. The composition contains a specific ethylene / α-olefin / non-conjugated polyolefin copolymer copolymer, a SiH group-containing compound having at least two SiH groups in one molecule, and optionally a catalyst and a reaction inhibitor. And the crosslinking rate at 160 ° C. (t c (90)) is 15 Minutes or less. The anti-vibration comb product and the glass run product of the present invention comprise the above composition. [Effect] The above composition has a high crosslinking rate and excellent productivity, and has a high HA Hot air cross-linking of V, UHF, etc. is possible, and the cross-linking agent does not flatten on the product surface, so it has excellent product appearance, It is possible to produce an environmentally friendly crosslinked rubber molded article having excellent compression set resistance and heat aging resistance and not releasing nitrosamine compounds at low cost. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2002146133-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2004031609-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005298593-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2015193680-A |
priorityDate | 1999-07-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 346.