http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2001019809-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_afea2aa6f1f892c1456cf7d7a8bc0242 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08L23-04 |
filingDate | 1999-07-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_33227dc2298abded0b53cd3ef5960a86 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a73e2e0290d107c99090c45a76ffc1f5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_a1893809a9a9db1f15fc4c95b9394f58 |
publicationDate | 2001-01-23-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2001019809-A |
titleOfInvention | Composition for packaging film, method for producing the same, and packaging film produced by the method for producing the same |
abstract | PROBLEM TO BE SOLVED: To provide a packaging film which is excellent in adhesiveness and can maintain adhesiveness for a long period of time, and a method for easily producing the same using an existing processing machine. SOLUTION: A packaging film composition is prepared by adding 2 to 25 parts by weight of the following resin modifying masterbatch composition to 100 parts by weight of a polyolefin resin, and a packaging film is obtained using the composition. 100 parts by weight of: (A) 30 to 95% by weight of low-crystalline polyolefin and (B) 5 to 70% by weight of polyisobutylene having a specific viscosity average molecular weight; (C) A masterbatch composition for resin modification obtained by kneading 1 to 50 parts by weight of a polyolefin having a melting point sufficiently lower than that of the polyolefin of (A) in a specific temperature range. |