Predicate | Object |
---|---|
classificationCPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C01B33-16 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/C08K9-06 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08K9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C01B33-159 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C1-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09C3-12 |
filingDate | 1998-02-18-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationDate | 2000-10-03-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000512972-A |
titleOfInvention | Hydrophobic organosilicate modified silica gel |
abstract | (57) [Summary] The present invention is a hydrophobic organosilicate-modified silica gel and a method for producing the same. The process of the present invention comprises two steps, in which the organosilicate modified silica hydrosol is heat treated at a pH of less than 1 in the presence of a strong mineral acid to form an organosilicate modified silica hydrogel. In a second step, the organosilicate-modified silica hydrogel was contacted with an organosilicon compound in the presence of a catalytic amount of a strong acid to achieve the hydrophobization of said organosilicate-modified silica hydrogel and thereby measured dry. to form a hydrophobic organosilicate-modified silica hydrogel having a surface area in the range of 100m 2 / g~750m 2 / g when. In a preferred method, the hydrophobic organosilicate-modified silica hydrogel is contacted with a sufficient amount of a water-immiscible organic solvent to convert the hydrophobic organosilicate-modified silica hydrogel into a hydrophobic organosilicate-modified silica organogel. . |
priorityDate | 1997-02-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |