abstract |
(57) [Summary] [Purpose] To provide an easily disintegrating moisture-proof paper which has no adverse effect on products such as coated paper, has excellent blocking resistance with more types of products, and has recovered recovered paper. thing. [Structure] On at least one side of a paper substrate, 1 to 20 parts by weight of wax and 100 parts by weight of synthetic resin in terms of solid content, average particle size A moisture-proof layer containing 0.1 to 50 parts by weight of an organic pigment of 5 to 70 μm is provided. |