http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000343599-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J5-18 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01G4-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C55-12 |
filingDate | 1999-06-07-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_3d535868cc547522ce61877411519b9c http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7c9efbe008c98c6114a13f67c7ed899b http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1ce55ce0941cd406b6f49100c4088cca |
publicationDate | 2000-12-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000343599-A |
titleOfInvention | Polyester film |
abstract | (57) [Problem] An object of the present invention is to provide a film suitable for a dielectric of a film capacitor having excellent insulating properties and workability. SOLUTION: The present invention comprises a biaxially stretched film containing polyethylene-2,6-naphthalenedicarboxylate as a main component, and the film has a center line average surface roughness (Ra) of 40 to 90 nm and a 10-point average. Roughness (Rz) 1000 to 1800 nm, 40 present in the film the number of coarse particles exceeding μ is 10 / m 2 or less; The heat shrinkage in the machine direction (MD) after treatment at 200 ° C. for 10 minutes is 0.9-3.0%, and the heat shrinkage in the transverse direction (TD) is 2.0-5.0%. Characteristic polyester film for capacitors. |