http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000340855-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_44b2ac87aeadb161b83426d9cf6c4bdc |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L41-297 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-49 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L41-22 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B35-493 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/H01L41-107 |
filingDate | 1999-05-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e29013aa74ebd8ca540423253429edce http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_dcfd1f19676b274d31a1ab644db06f5e |
publicationDate | 2000-12-08-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000340855-A |
titleOfInvention | Piezoelectric ceramic device |
abstract | (57) [Problem] To provide a piezoelectric ceramic device capable of preventing delamination of a palladium electrode even at low temperature firing. An internal electrode containing palladium as a main component is provided. A piezoelectric ceramic device 1 which is fired at a temperature of 1150 ° C. or less, wherein more than 1% by weight and less than 10% by weight of glass is added to an internal electrode with respect to a metal component contained in the internal electrode 102. ing. |