http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000328360-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-84 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F6-92 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/D01F1-10 |
filingDate | 1999-05-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_49322e4bbaf73315e624099d39033278 |
publicationDate | 2000-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000328360-A |
titleOfInvention | Polyester fiber |
abstract | (57) [Summary] [PROBLEMS] To reduce the occurrence of thread breakage and wrap during stretching without reducing the stretching speed and the stretching ratio without containing titanium oxide, and to stably produce the yarn. Providing high polyester fiber. SOLUTION: The polyester containing ethylene terephthalate as a main repeating structural unit, wherein a dicarboxylic acid component other than terephthalic acid and / or a glycol component other than ethylene glycol is 0.1 to 5.0 based on the terephthalic acid component. 0.001 to 0.2 parts by weight of an alkaline earth metal salt of sulfuric acid and / or an alkaline earth metal salt of carbonic acid are added to 100 parts by weight of a polyester which is mol% copolymerized and does not contain titanium oxide. A polyester fiber obtained by melt-spinning a polyester composition. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/CN-101046007-B |
priorityDate | 1999-05-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 41.