http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000328005-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_f1192a135e4bc40a5f201a9646f20172 http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_0a521cfa321c963978df8ae98a84056a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C09D183-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-24 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D7-14 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B05D5-00 |
filingDate | 1999-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0e52e80d6e253af435b60833073a7829 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_57e554500cbc4c22899b2d11f38eba8a http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7c00e33215d3d5276e96f4cd59e791ae http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_9b28545dc29e0ba04efb6bc774c20542 |
publicationDate | 2000-11-28-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000328005-A |
titleOfInvention | Stain resistance treatment method for top coat |
abstract | (57) [Summary] [PROBLEMS] To impart a stain resistance function to the outermost surface of a coating film regardless of the type and history of the top coating film, and to maintain a clean coating film for a long period of time. To provide a stain-resistant treatment method for a top coat capable of maintaining the above performance even when light is blocked for a long period of time. The component (a) has the formula: R 1- (OCH 2 CH 2 ) n -O —Si (OR 2 ) 3 (where R 1 is an alkyl group having 1 to 6 carbon atoms or a hydrogen atom, R 2 is an alkyl group having 1 to 6 carbon atoms, and three R 2 are the same or different. N: an integer of 1 to 4), or 100 parts by weight of a partially hydrolyzed condensate thereof and a component (b): a catalyst capable of hydrolyzing the component (a) A method for treating stain resistance of an overcoat film, comprising applying a mixture consisting of 0.01 to 5 parts by weight to the overcoat film and then subjecting the mixture to hydrolysis treatment. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2009066141-A1 |
priorityDate | 1999-05-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |