http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000302856-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_696ca0ae93d5cf5a686273601361781f |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B7-24047 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G11B7-2534 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G64-04 |
filingDate | 1999-04-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_68f07988b31453a9d2d465fec0fbb616 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_977c9661bd35856c84b8550aed9758b1 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_6e42b8f6c2d2fa0d4259be7be809f5a9 |
publicationDate | 2000-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000302856-A |
titleOfInvention | Molding material for optical recording media |
abstract | PROBLEM TO BE SOLVED: To provide a molding material for an optical recording medium having excellent moldability and low birefringence. SOLUTION: An intrinsic viscosity obtained by reacting bis (4-hydroxyphenyl) diphenylmethane, a compound having a phenolic hydroxyl group having three or more functional groups with a bisphenol of the general formula (1), and a carbonate-forming compound is 0.1. A molding material for an optical recording medium comprising polycarbonate having a weight of 30 to 0.50 dl. Embedded image |
priorityDate | 1999-04-19-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Predicate | Subject |
---|---|
isDiscussedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/substance/SID226422970 http://rdf.ncbi.nlm.nih.gov/pubchem/compound/CID232881 |
Total number of triples: 16.