Predicate |
Object |
assignee |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_7ef01e33058cf740cf2197991be97af1 |
classificationIPCInventive |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29B13-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-88 |
filingDate |
1999-04-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor |
http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_05c3babfef994d17f6113cafc7669952 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_1e9325454be207f4f10056b24346c9f5 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_b6b91791e9aed5917903717f639018bc http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_747f0f88b77e6ccec0135dda4d4d48a0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7faad4c63320cd9ae7d8459726bb46c0 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8a3009bc5e149cc9aa70132fc9eb9ce8 |
publicationDate |
2000-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber |
JP-2000302855-A |
titleOfInvention |
Crystallization method of aliphatic polyester |
abstract |
(57) Abstract: A crystallization method in which an aliphatic polyester in a solid state is crystallized by contact with a liquid. A crystallization method in which a molten aliphatic polyester is solidified and crystallized by contact with a liquid. A crystallization method in which an aliphatic polyester solution obtained by dissolving an aliphatic polyester in a solvent is brought into contact with a liquid to solidify and crystallize the solution. [Effect] When crystallizing aliphatic polyester, Crystallization can be performed without being restricted by the molecular weight or the relative viscosity η rel and without causing problems such as fusion and breakage. By crystallizing the aliphatic polyester, stable operation can be performed without problems such as fusion of particles, breakage of particles, and blockage in the device. In crystallization of the aliphatic polyester, crystallization can be performed at a lower temperature and in a shorter time than conventional crystallization methods without fusing or breaking. |
isCitedBy |
http://rdf.ncbi.nlm.nih.gov/pubchem/patent/US-7728100-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-4693346-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-5234585-B2 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2004107457-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2005126490-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/KR-20030067867-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/DE-102005008115-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2007034805-A1 |
priorityDate |
1999-02-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type |
http://data.epo.org/linked-data/def/patent/Publication |