http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000302511-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_82d2433d950fca4901936ab9e6f91c40 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B26-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C04B14-02 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/E04G23-02 |
filingDate | 1999-04-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_92b95c918af29f4a18d0efd880125720 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_7acc968b7025241d64c9a56ab79eff94 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_87bfb8992b5442b9dd4bbc706e81502b |
publicationDate | 2000-10-31-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000302511-A |
titleOfInvention | Repair material for concrete |
abstract | (57) [Summary] [Problem] To replace the cement contained in a repair mortar or repair material with a material that is substantially the same and inactive as cement, thereby reducing the efflorescence phenomenon during or after repair of concrete. Provided is a concrete repair material that can prevent the repaired part from having the same texture and color tone as the concrete around it while preventing the repair. A repair material for concrete, which is filled in a defective portion of concrete and used for repairing the concrete, includes: a crushed rock having a particle size of 300 μm or less; It is a concrete repair material containing a gray amorphous substance of m or less and a synthetic resin emulsion or a synthetic rubber latex. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2013087596-A |
priorityDate | 1999-04-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 30.