http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000296695-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_4e1451b5c6ae6723eb5cefa99e5d1b9b |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/A47B97-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B43L3-00 |
filingDate | 1999-04-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_bd592d16ae6691f5bc3fbedf4fc18b66 |
publicationDate | 2000-10-24-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000296695-A |
titleOfInvention | Desk mat |
abstract | (57) [Summary] [Problem] A conventional vinyl chloride desk mat generates dioxin when incinerated, and the olefin resin desk mat has a reduced transparency when subjected to a graining process to make scratches less noticeable. SOLUTION: The desk mat of the present invention has a core material 1 made of an ethylene-based resin or an elastomer based on the same. A protective layer 3 is formed by laminating an ethylene-vinyl alcohol copolymer on both front and back surfaces of the protective layer 3 via an adhesive layer 2 made of an adhesive resin or an adhesive. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2022024168-A http://rdf.ncbi.nlm.nih.gov/pubchem/patent/WO-2017212310-A1 |
priorityDate | 1999-04-14-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 21.