http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000292879-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_13aa7b32ae00ed83af7dfaa0b6a1f7c2 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-30 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-26 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C5-08 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C11-00 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-00 |
filingDate | 1999-04-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_972adfcaaf157f8989ef72eb72400737 |
publicationDate | 2000-10-20-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000292879-A |
titleOfInvention | Image forming method |
abstract | PROBLEM TO BE SOLVED: To provide an image forming method for a silver halide photographic light-sensitive material for printing plate making, which has an ultra-high contrast and is excellent in dot quality, even in rapid processing with a short exposure time and a short processing time. provide. SOLUTION: At least one silver halide emulsion layer is provided on a support, and the silver halide emulsion layer or the non-photosensitive hydrophilic colloid layer contains at least one hydrazine derivative in an amount of 1 × 10 −5 to 1 × 10 5. In a method for forming an image having a concentration of 4.5 or more by exposing a silver halide photographic light-sensitive material containing -3 mol / m 2 to an image setter and then processing the same with an automatic developing machine, the exposure energy at the time of exposure is reduced. 0.01 ~ 10 μJ / (sec · cm 2 ), exposure time 5 × 10 −7 11 × 10 -10 seconds, and at the time of processing, the following general formula (B) An image forming method comprising processing using a processing agent containing a compound represented by the formula (I) as a developing agent and containing substantially no hydroquinone derivative. |
priorityDate | 1999-04-12-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |