http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000290423-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_33dafb5bbc2ec47ebcb7becbbe60f704 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B29C41-12 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-28 |
filingDate | 1999-04-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_133d1c5e437be25904be2dc9597b8be9 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ce1332b145194fe2387b1a586d049206 |
publicationDate | 2000-10-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000290423-A |
titleOfInvention | Method for producing ethylene-vinyl alcohol-based porous membrane |
abstract | PROBLEM TO BE SOLVED: To provide a production method capable of easily obtaining an ethylene-vinyl alcohol-based porous membrane having extremely excellent water permeability as compared with a conventional ethylene-vinyl alcohol-based copolymer membrane. To do. A temperature T1 containing an ethylene-vinyl alcohol-based copolymer and a solvent defined by the formula (1) as main components. Is cooled to T2 at an average cooling rate of 200 ° C./sec or less after film formation, or formed into a film while cooling to T2 at an average cooling rate of 200 ° C./sec or less, and then the solvent is removed. It is achieved by doing. a / b ≧ 10 and b ≦ 1% by weight (1) (where a is the solubility of the ethylene-vinyl alcohol copolymer in the solvent at the temperature T1, and b is the temperature T 2 is the solubility of the ethylene-vinyl alcohol copolymer in the solvent. However, 30 ° C ≦ T1 ≦ 250 ° C, −10 ° C ≦ T2 ≦ 60 ° C, T2 + 10 ≦ T1 |
priorityDate | 1999-04-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 36.