http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000290362-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_1374dd16777534b65ad4422333245af8 |
classificationCPCAdditional | http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02W30-62 http://rdf.ncbi.nlm.nih.gov/pubchem/patentcpc/Y02P20-143 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J11-04 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08G63-91 |
filingDate | 1999-04-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_cb88dd14bc29d4bc23638249bd4a2864 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_2dccd441842478bbb5bdd6ce42f0c621 |
publicationDate | 2000-10-17-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000290362-A |
titleOfInvention | Recycling method of polyester molded product |
abstract | (57) [Problem] To provide a polyester product having the original heat resistance and mechanical properties of a polyester even if it contains organic impurities when a molded product made of a polyester polymer is used as a recycled product. To provide a method for reclaiming molded articles. SOLUTION: Organic impurities are at least 0.01% by weight. A method for regenerating a molded article comprising a polyester polymer, comprising reacting the polyester polymer with 0.01 to 3% by weight of a bisoxazoline compound represented by the following structural formula based on the molded article: The intrinsic viscosity of the polyester polymer is 0.5 to 1.1. |
priorityDate | 1999-04-09-04:00^^<http://www.w3.org/2001/XMLSchema#date> |