http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000284417-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-498 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-76 |
filingDate | 1999-03-30-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e11a5c1fd4267df3ca10da3d3b879be4 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_e56a63e0ac2d7d2db0e82acea5362fb0 |
publicationDate | 2000-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000284417-A |
titleOfInvention | Heat-developable image forming material |
abstract | (57) [Problem] To provide a photothermographic material, particularly a photothermographic material, in which cracks are prevented from occurring during thermal development. SOLUTION: The coefficient of thermal expansion on a support is 1.0 to 1.5. It has at least one heat-developable image-forming layer below, has a coefficient of thermal expansion of 0.9 or more and less than 1.0 above the heat-developable image-formed layer with respect to the support, and has a glass transition temperature of A heat-developable image-forming material having a layer using at least one polymer latex having a development temperature or lower. |