http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000284399-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_03d0f52bb4069f8a19d70dcfb697c67a |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/G03C1-498 |
filingDate | 1999-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_0e828954a7196af00aba78f394221cca http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_ea7a4ad0394ab3db2f59c1029e1efd42 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_8d5bf105711ba600671d491960ef9b21 |
publicationDate | 2000-10-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000284399-A |
titleOfInvention | Photothermographic material |
abstract | (57) [Summary] [PROBLEMS] Particularly for photoengraving, especially for scanners and imagesetters, it is super-hard, hard to fog, does not generate black spots, and has good Dmax (maximum density) and halftone dot quality. To provide a photothermographic material capable of obtaining an optimum image for photolithography. SOLUTION: In a photothermographic material having a non-photosensitive silver salt, a photosensitive silver halide and a binder on a support, a nucleating agent is contained on the support having a photosensitive silver halide, and Silver content of formic acid or formate A photothermographic material characterized in that the amount is 5 mmol or less per mole. |
isCitedBy | http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1582919-A1 http://rdf.ncbi.nlm.nih.gov/pubchem/patent/EP-1635216-A1 |
priorityDate | 1999-03-29-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links
Total number of triples: 492.