http://rdf.ncbi.nlm.nih.gov/pubchem/patent/JP-2000281828-A
Outgoing Links
Predicate | Object |
---|---|
assignee | http://rdf.ncbi.nlm.nih.gov/pubchem/patentassignee/MD5_24aca9ded2638ea793d05360dde7a4a0 |
classificationIPCInventive | http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/C08J9-06 http://rdf.ncbi.nlm.nih.gov/pubchem/patentipc/B32B5-18 |
filingDate | 2000-01-13-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
inventor | http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_c1903d0ff51d30727a2fc41a8c717f50 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_d46a3340a78577c51b3cb349cca44751 http://rdf.ncbi.nlm.nih.gov/pubchem/patentinventor/MD5_50ad106ffe511571b6ca7f48166dc65a |
publicationDate | 2000-10-10-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
publicationNumber | JP-2000281828-A |
titleOfInvention | Polymer composition for powder foam molding |
abstract | PROBLEM TO BE SOLVED: To contain a polymer containing an epoxy group as one component, to provide excellent storage stability of an uncrosslinked composition, to enable crosslinked foaming in a short time, and to set compression set. Provided is a polymer composition for powder foam molding capable of providing a foam which is small in size, has excellent surface skin, and has almost no skin ding, a powder, a foam using the composition, a method for producing a foam, and a molded article. . SOLUTION: The polymer (A) containing an epoxy group, 1 A peroxide (B) having a temperature of 100 ° C. or higher for obtaining a half-life of 0 hour, at least one of quaternary ammonium salts and quaternary phosphonium salts (C), and a pyrolytic foaming agent (D) A polymer composition for powder foam molding comprising: |
priorityDate | 1999-01-27-04:00^^<http://www.w3.org/2001/XMLSchema#date> |
type | http://data.epo.org/linked-data/def/patent/Publication |
Incoming Links